Time-Dependent Flexural Behaviour of Reinforced and Prestressed Alkali-Activated Concrete

Doctoral Thesis (2026)
Author(s)

Z. Qian (TU Delft - Civil Engineering & Geosciences)

Contributor(s)

M. Lukovic – Promotor (TU Delft - Civil Engineering & Geosciences)

G. (Guang) Ye – Promotor (TU Delft - Civil Engineering & Geosciences)

E.O.L. Lantsoght – Copromotor (TU Delft - Civil Engineering & Geosciences)

Research Group
Concrete Structures
DOI related publication
https://doi.org/10.4233/uuid:ee181d72-93eb-459d-9a0c-74270cabc7b2 Final published version
More Info
expand_more
Publication Year
2026
Language
English
Defense Date
02-10-2026
Awarding Institution
Delft University of Technology
Research Group
Concrete Structures
ISBN (print)
978-94-6518-453-1
Page Views
30
Reuse Rights

Other than for strictly personal use, it is not permitted to download, forward or distribute the text or part of it, without the consent of the author(s) and/or copyright holder(s), unless the work is under an open content license such as Creative Commons.

Abstract

Alkali-activated concrete (AAC) is a promising sustainable alternative to Portland cement concrete (PCC), as it can reduce the environmental impact associated with cement production. However, the structural behaviour of AAC members, especially prestressed members, remains unknown. Certain AAC mixtures, especially those made from high-calcium precursors, can exhibit reduced mechanical properties under drying, along with significant shrinkage and creep, affecting the long-term performance of AAC structural members. The primary aim of this thesis is to investigate the time-dependent flexural behaviour of reinforced and prestressed AAC members, focusing on the influence of curing/exposure conditions.
Material and structural behaviour of self-compacting AAC (SCAAC) was tested. The material tests showed that SCAAC was sensitive to drying. Exposure to drying led to decrease in splitting tensile strength and elastic modulus, while under continuous moist curing, compressive strength, splitting tensile strength and elastic modulus of SCAAC increased or remained constant. The reduction is attributed to drying-induced microcracking and carbonation. Free shrinkage and creep of SCAAC continued to increase over approximately 3 years and 1 year, respectively. Unlike SCAAC, the strength and elastic modulus of the reference PCC mixture increased or remained constant under drying.
Flexural behaviour of reinforced SCAAC beams was investigated at different testing ages. Drying-exposed SCAAC beams showed decrease in cracking load and stiffness over time, as well as larger maximum crack widths than the 28-day beam. Slightly smaller crack spacing was observed in drying-exposed SCAAC beams tested at later ages, which was not captured by the existing analytical models. The performance of moist-cured SCAAC beams and reference drying-exposed PCC beams was almost constant over time. The changes in the flexural behaviour of drying-exposed SCAAC beams were partially attributed to the evolution of elastic modulus and tensile strength. The shrinkage effects in reinforced beams also contributed to reductions in cracking load and stiffness, and to the increase in crack width. Considering these effects improved the analytical predictions of the flexural behaviour of drying-exposed SCAAC beams.
The time-dependent flexural behaviour of composite AAC girders comprising a precast prestressed girder and cast-in-situ topping, a common composite construction system in the Netherlands, was also studied. The experimental programme included 28-day flexural tests, deflection measurements of two specimens subjected to self-weight and additional sustained loading over 9 months, and subsequent flexural tests at 9 months. Similar to reinforced SCAAC beams, the 9-month composite girders exhibited reduced stiffness, decreased cracking load and larger crack widths compared to the 28-day specimen. The lower cracking load arose from prestress losses due to ongoing shrinkage and creep. Larger crack widths indicate a reduction of bond between AAC and prestressing strands over time. Distinct failure patterns were found in the 9-month specimens: anchorage failure for specimen subjected to self-weight only and flexural failure for specimen exposed to additional sustained load. This highlights the role of creep on the bond behaviour between prestressing strands and AAC, particularly as a function of varying stress at the level of strands. The prestress losses could be predicted analytically once the effects of restrained deformation (i.e. creep and shrinkage) between the precast girder and topping AAC were considered.
A numerical study was performed to investigate the influence of drying on the time-dependent behaviour of AAC. A staggered lattice modelling approach, combining lattice moisture and lattice fracture models, was applied to simulate moisture exchange, drying shrinkage-induced fracture, and fracture behaviour under external load. The simulations showed that drying led to concrete cracking, development of steel stresses, and bond reduction, thereby reducing the cracking load and stiffness of reinforced beams over time. The model could well reproduce the experimental observations and provide further insights into shrinkage-induced stresses and damage.
This thesis addresses the knowledge gap regarding the long-term behaviour of AAC under exposure to drying (i.e. 20 ℃ and 50% RH). The study reveals that, for the investigated high-calcium AACs, 28-day tests do not provide a safe reference for design. The testing methods, including curing/exposure conditions before testing, and the analytical models used for PCC cannot be unconditionally adopted. Unlike for PCC, 28-day compressive strength cannot provide a safe reference for the design of AAC exhibiting pronounced time-dependent behaviour. Elastic modulus is more sensitive to internal changes (e.g. microcracking) and therefore can provide better insight into the long-term behaviour of AAC. The influence of restrained shrinkage and creep should be considered for structural members produced by such AAC.
Building on the obtained knowledge, recommendations are provided for mixture design and curing conditions, key tests, prediction methods and post-construction monitoring. These recommendations can further be adapted to other AAC mixtures and boundary conditions after validation and therefore provide a basis for developing more general guidance for AAC applications.