Isothermal heat treatments below the martensite start temperature are carried out in a 0.25C-1.4Mn-1.4Si-0.32Mo steel (in wt%). The microstructural observation reveals a combination of tempered lath and plate martensite, accompanied by bainite and retained austenite. The temperat ...