In situ assessment of the reuse potential of fully toughened glass

Journal Article (2026)
Author(s)

Pascal Mobailly (Student TU Delft)

Rebecca Hartwell (École Polytechnique Fédérale de Lausanne)

Chris Noteboom (Advies- en Ingenieursbureau van de Laar B.V.)

Mitsu Edwards (Eckersley O’Callaghan)

Christian Louter (TU Delft - Civil Engineering & Geosciences)

Research Group
Applied Mechanics
DOI related publication
https://doi.org/10.1007/s40940-026-00337-3 Final published version
More Info
expand_more
Publication Year
2026
Language
English
Research Group
Applied Mechanics
Journal title
Glass Structures and Engineering
Issue number
3
Volume number
11
Article number
25
Page Views
33
Reuse Rights

Other than for strictly personal use, it is not permitted to download, forward or distribute the text or part of it, without the consent of the author(s) and/or copyright holder(s), unless the work is under an open content license such as Creative Commons.

Abstract

Architectural glass is among the most energy-intensive construction materials to produce. Yet, a significant portion of end-of-life glazing is down-cycled or landfilled at low environmental value. In the best case scenario, glazing products are crushed at the end of their service life and recycled into cullet for new float glass: direct reuse of glass panes is seldom considered. One of the primary obstacles to the reuse of glass panes is the uncertainty in the residual strength of aged glass. Efficient test protocols are required to provide an enhanced understanding of the post-aged strength of glass. In this work, a non-destructive optical testing approach is presented to estimate the strength of aged glass in situ, based on measurements of pre-stress and surface flaw characteristics, and combined with a life-cycle assessment to analyse the environmental impact modelled through alternative end-of-life scenarios. This approach was applied to a sample of 70 fully thermally toughened monolithic glass panes that were over 50 years old, inside a historic building in Paris. The measured surface compressive pre-stress averaged 81.41 MPa with a standard deviation of 4.17 MPa, and maximum flaw depths ranged from 4 to 147 μm. Based on these findings, a classification system is proposed that links the visual inspection procedure with characteristic strength values. Through the newly developed classification system, all 70 tested panes are found to meet the characteristic design strength associated with heat-strengthened applications, and are therefore deemed suitable for structural reuse. For the 2464 panes, in situ reuse gives a total life-cycle GWP of 15.3 and 85.6 tonnes CO2-e at reuse yields of 95% and 72% respectively, compared with 215.9 tonnes for a closed-loop recycling scenario and 301.8 tonnes for current down-cycling and landfill practice. The findings suggest that a combined techno-environmental assessment can support the rapid on-site evaluation of flat glass panes and facilitate their reuse.